Imininingwane Yemikhiqizo
Incazelo: Ishidi le-graphite eliguquguqukayo lenziwa nge-graphite enwetshiwe emsulwa. Ishidi le-graphite lomkhiqizo we-"Sungraf" linokuhlanzeka okuphezulu kokuqukethwe kwekhabhoni okungu-99%.
Izinzuzo
ukumelana okungcono kwamakhemikhali, ukuguquguquka okungcono kwe-thermal, nokuvaleleka okungcono.
Ukusetshenziswa
- 01 Njengempahla ye-gasket, imvamisa yenziwa ibe yi-Graphite Laminate, ishidi le-graphite eliqinisiwe
- 02 esetshenziswa kabanzi ezinhlelweni zokuvala uketshezi: i-flange gasket, i-spiral ulcer gasket, i-heat exchanger gasket, njll.
- 03 Ingasetshenziswa futhi njengesithambiso esiqinile ekunyatheleni izitembu zensimbi nasekwakheni izinhlelo zokusebenza, noma njengolayini wokushisa eziko ezimbonini nakwezinye izinto zokushisisa.
Usayizi
Uhlobo | Ubukhulu (mm) | Ububanzi (mm) | Ubude(mm) |
KumaSpredishithi | 0.2-6.0 | 1000, 1500 | 1000, 1500 |
KumaRoll | 0.2-1.5 | 1000, 1500 | 30m-100m |
Izakhiwo Zobuchwepheshe: (Izici Ezikhethekile zihlangabezana nezidingo zamakhasimende.)
SGM-A | SGM-B | I-SGM-C | I-SGM-CC | |
Okuqukethwe kwekhabhoni (%) | 99.5 | 99.2 | 99.0 | 99.0 |
Okuqukethwe kwesibabule (PPM) | 200 | 500 | 1000 | 1200 |
Okuqukethwe kwe-Chloride (PPM) | 20 | 30 | 40 | 50 |
Ukubekezelela Ukuminyana (g/cm3) | ±0.03 | ±0.03 | ±0.04 | ±0.05 |
Ukubekezelela Okujiyile (mm) | ±0.03 | |||
Amandla Okuqina (Mpa) | ≥4.0 | |||
I-Compressibility (%) | ≥40 | |||
Ukubuyisela (%) | ≥10 |
I-SGM-C Flexible graphite sheet Data Technical
Ukuminyana | 1.0g/cm3 |
Okuqukethwe kwekhabhoni | 99% |
Okuqukethwe Umlotha ASTM C561 | ≤1% |
I-Chloride etholakalayo ye-ASTM D-512 | 50ppm Max. |
Okuqukethwe Kwesibabule ASTM C-816 | 1000ppm Max. |
Okuqukethwe kweFluorides ASTM D-512 | 50ppm Max. |
Izinga Lokushisa Lokusebenza | -200 ℃ kuya ku-+3300 ℃ I-Non-Oxidizing -200 ℃ kuya +500 ℃ Oxidizing -200 ℃ ukuya +650 ℃ I-Steam |
Ingcindezi | 140bar Max. |
Amandla Okuqina | 998psi |
I-Stress Relaxation DIN 52913 | 48N/mm2 |
I-Creep Relaxation ASTM F-38 | <5% |
I-Compressibility ASTM F36A-66 | 40 - 45% |
Ukubuyisela i-ASTM F36A-66 | ≥20% |
Ukulahleka Kokuthungela | Ngaphansi kuka-1%(450℃/1Hr) Ngaphansi kuka-20%(650℃/1Hr) |
Ukuvaleleka kwe-ASTM F-37B uphethiloli A | <0.5ml/h |
Ukumelana Nogesi | 900 x 10-6 ohm cm ngokuhambisana nendawo 250, 000 x 10-6 ohm cm Perpendicular to surface |
I-Thermal Conductivity | 120 Kcal/m Hr. ℃ parallel to surface 4Kcal/m Hr. ℃ Perpendicular to surface |
Ukunwetshwa kwe-Thermal | 5 x 10-6 /℃ parallel to surface 2 x 10-6 /℃ Perpendicular to surface |
I-Frictional Coefficient | 0.149 |
PH | 0-14 |